① Chemical composition (ASTM A240, %)

Main alloying elements (scale 0–25%)
Cr
18.0–20.0 Corrosion resistance
Ni
8.0–10.5 Austenite stabiliser
Mn
≤2.00 Nickel substitute
ElementRange
C≤0.08
Si≤0.75
Mn≤2.00
P≤0.045
S≤0.030
Cr18.0–20.0
Ni8.0–10.5

② Mechanical properties (ASTM A240)

PropertyRequirement
Tensile strength Rm≥ 515 MPa
Yield strength Rp0.2≥ 205 MPa
Elongation A≥ 40%
Hardness≤ 201 HBW

③ Available sizes (standard range)

  • Thickness: 0.3–60 mm
  • Width: ≤ 2000 mm
  • Form: coil / sheet / plate / circle / slit strip on request
  • Surface: 2B · BA · No.1 · No.4 · HL · 8K on request

④ Applicable standards

ASTM A240 · EN 10088-2 · JIS G4304/4305 · GB/T 3280

⑤ Typical applications

Cookware, appliance panels, elevator trim, curtain walls, food equipment, tanks, flanges

⑥ Substitution and selection advice

General-purpose first choice. Choose 304L if welded assemblies must resist sensitisation; 316L for chloride pitting resistance; 201 only for dry indoor cost-down.

Chemical and mechanical data quoted from the public ASTM A240 standard. Available sizes are standard ranges; the contract and technical agreement prevail.